The vertical position of the chips leads to the following technical characteristics:
1. Thickness swelling
- low production tolerance
- very low thickness swelling during storage
- therefore sanding is not necessary
Advantages for door manufacturing :
- smooth surface
- Multi-Layer-Cores possible
- optimal conditions at the door press
2. Compression resistance
- high compression resistance
Pressing power during further processing causes no problems, even not when using strips of tubular board - high shock resistance.
ideal for ‘hard body’-performance
3. Bending Strength
- mostly lower than of flat pressed boards
Extruded boards are used as cores or middle layers. They are always crossbanded on both sides with thin particle board, hardboard, MDF or plywood. In all cases the bending strength is obtained by crossbanding.